-----Removing Chrome and Cadmium from Ground Water
How to remove cadmium and hexavalent in groundwater contaminate, before distribution to commercial area, most effective way ?
Kulchaya Tanongstudent - Bangkok, Thailand
September 17, 2008
September 25, 2008
Hi, Kulchaya. I assume this is a scholastic project. Ion exchange has been used for removal of hexavalent chromium in groundwater. Depending on the concentration of cadmium you might want to try chemical precipitation before the ion exchange. Both of these materials are toxic and must be reduced to the ppb range.
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
Thank you very much!
Kulchaya Tanong- Bangkok, Thailand
June 1, 2009
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.