Does black oxidizing change the thickness of a part?

 

September 24, 2008

We recently just made some parts and send them out to be black oxidized. Will this coating change the thickness of the part? thanks

Ben Knight
engineer - Birmingham, Alabama
  ^- Privately contact this inquirer -^
September 24, 2008

No, Ben, it won't. The thickness is measured in millionths of an inch rather than ten thousandths or thousandths.

Regards,

pic of Ted Mooney Teds signature
Ted Mooney, P.E.
finishing.com
Brick, New Jersey


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search