Home of the finishing HOTLINE since 1989

-----

What is Anticorrosive to Chromic Acid in Bath




September 22, 2008

Dear sir,

I need to find about chemical to anticorrosive in chromic bath. My friend recommend fluoro type from Dupont. Do you have recommend any chemical or company is made it to me?
Thank for your kindly in advance and looking forward to your reply soonest.
Best Regards,

Anirut Fuengrabilchoke
Trading - Dysit, Bangkok, Thailand



September 23, 2008

Hi, Anirut. It's not clear to me what you are looking for. A tank lining or heating coil that is resistant to chrome? Yes, teflon and several other fluoro type plastics are resistant. For tank linings, PVC is not fully resistant but is adequate. Or perhaps you're looking for a fluorinated fume suppressant?

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.





Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"