Process for silver plating of flange nuts
September 15, 2008
We have some requiremnts of Silver plating of flange nuts ,the thread portion only.
I am looking for a good process to put in use.
Fastener Manufacturer - Chennai,India
^- Privately contact this inquirer -^
September 18, 2008
Hi, Narisimhan. You will probably need to mask everything but the thread, and then silver plate.
It is not impossible to rig up moveable masks in some sort of a bandolier/belt system, but it would involve significant costs, and only be applicable for very large volume.