Home of the finishing HOTLINE since 1989

-----

Is 7075 Aluminum compatible with Limonene?


I am an engineering student at Lafayette College in Easton, PA.

I am trying to make traps in a Carbon Monoxide system that will be cooled by limonene. The traps are to be made with aluminum. If we submerge the aluminum bodied traps into a tank of limonene will the traps corrode?

Jeffery Taterson
student - Easton, PA, USA
August 14, 2008


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"