Corrosion resistant black finish for Bronze
[California]
July 14, 2008
We are seeking a finish for a silicon bronze casting - an
enclosure for an underwater floodlight. We would like a dull black
color similar to black oxide on steel. What is a similar blacking
process that can be used on a silicon bronze casting (alloy CA873)?
Ben Gallant