49092
Rechroming automotive parts with welded lap
joint
June 22, 2008
Dear friends, firstly, thank you for your time and good advice on
the forum.
It is true that steel parts that are stripped of decorative chrome
and then re-plated will tend to rust in areas where two parts,as with
a spot welded lap joint, are in close contact ? Every plant that I
have taken my parts to has told me that this is an unavoidable side
effect from when the original chrome was stripped. Thanks for your
replies.
Jeremy Warren