Metal finishing Q&As since 1989


-----

Gold plating adhesion




Any past articles regarding adhesion of gold plating on crs steel. only requirement from customer is no under coatings (nickel strike etc..)can be used. thanks rv

Paul Bernardy
plating shop - Denver, Colorado, USA
June 3, 2008



June 5, 2008

Hi, Paul. Yes, use the search term 'gold strike' and you will find at least some general discussion about acid gold striking.

Regards,

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

 
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g, Train'g
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"