NICKEL SILICON PLATING
.
I AM IN SEARCH OF NICKEL SILICON OR NICASIL PLATING EQUIPMENT.I
PLAN ON USING THE EQUIPMENT FOR SMALL ENGINE CYLINDERS.ANY LEADS ON
THIS WOULD BE APRECIATED.
GARRY GODDEN
- SHADY COVE OR USA
.
Search the back issues of the hot line, about 6 months ago. There
were several replies to a letter similar to yours. It is a
proprietary process. If I remember correctly, the main one is in
England and there is one in Auburn,AL.
JamesWatts
- FL
.
Jim's reply motivated us. We've added Nikasil plating to our
FAQs page.
|
|