48079

Questions about Composite Diamond Coating  

March 6, 2008

I am doing a composite diamond coating on a parts of engine rotor. The electrolytic is Nickel Sulfamate. The coating area is like a screw with a wave through and peaks on circle. The diamond particles is 90 to 107 micro. Here are some question.

1. The specimen was buried into the diamond powder or suspension diamond powder, which one is adaption me condition?? or other way??

2. Do the powder need pre-treatment before add into the solution?? If yes, how to pre-treament??

3. Is the surfactant need??

Anymore suggestion for this case, please tell me.

Thanks

Philipa Lin
product designer - Taiwan





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com