Need to anodize magnesium parts - have 1000
pieces [California]
February 15, 2008
I need a plating house that can do this process . I have the full
spec
PLATE PER ASTM D1732, note MIL-M-45202 IS SS BY ASTM D1732
I have 1000 pieces that need this process
Shaun Tan