Is there White Anodize?
+++++++
It seems like every 10 years I get a customer coming to me with the same questions. This time it's "is there anything such as white anodize?" The last time I saw this was about 15 years ago when Lockheed Sunnyvale (priot to the Martin Marieta merger) sent out a request asking if anyone had a white anodize. I've been asked again and wonder if I've missed something. I've seen a nice hard eggshell white anodic coating on magnesium done using the Magoxid method but as far as aluminum goes, I've seen nor heard anything.
Milt StevensonPlating Shop Employee - Syracuse, New York
+++++++
Other letters 11600, 20562, 39842, and 41596 address this topic. It seems the answer is "close but no cigar".
|
Ted Mooney, P.E. finishing.com Brick, New Jersey |
January 14, 2008
Some years back a large finishing company that I worked for in the Springfield, Massachusetts area developed a very nearly white anodize. I'm not sure if they still offer it on a small run, custom basis. Large runs were definitely out of the question.
Tim HamlettDecorative Plating - North Miami, Florida, USA