46091
How can I do electroless deposition of
titanium?
+++++++
Dear Sir,
I am a researcher in National centre for catalysis research,
India. I would like to carry out electroless deposition of Ti on
various substrates. May anyone suggest me how to do the experiment.
Kindly suggest to me which Ti precursor is to be used.
Sincerely,
Balasundaram Murugan
Student - Chennai, Tamilnadu, India
+++++++
Your idea is interesting and as afar as I am aware has not been
done from an aqueous system. I am of the opinion that electoless
deposition of titamium in an aqueous environment is impossible. One
of the joys of being a student is discovering new things, so I would
suggest you develop your scientific knowledge of the properties of
titanium and its associated metals and try to develop a workable
process. If you decide to copy someone else's ideas and successes, it
doesn't make you a good scientist, just a simple copier - develop
your own successful process and then you become a scientist!
|
|
Trevor Crichton
R&D practical scientist - UK
|


 |