Dear Sir

What is the emission limit for open tanks during hardchrome plating?
Note that We are not using any fume suppressant in our tanks.
please help!!

Best Regards

Mohsin Siddiqui
Assistant Manager - Karachi, Pakistan


+++++++

Hi Mohsin,

The U.S. specs for chromic emissions are very tough, ie. 0.05 mg/cu M....maybe too tough.

The specs back in l978 in B.C. were ll grains of sulphuric/chrome per 1,000 cfm (or was it per single
cfm, I forget).

Using an ordinary but very well built CT-120/2 blade type eliminator, we achieved 0,34 grains .... that's equivalent to 30 times lower than those specifications BUT translated into metric, it's only O.7OO mg/cu.M Yes, I have that in writing.

You definitely need some exhaust.

Does this help?

Freeman Newton
- White Rock, B.C. Canada

Ed. note: Welcome back, Freeman, and get back to 100 percent soon.





Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com