-----Need Mil-C-5541 and Mil-A-8625 on Beryllium-Aluminum Castings
I'm looking for Plating House and would appreciate if you could provide us the lists of contacts and companies on the Surface Treatment services for Beryllium 63%/Aluminum 33% Castings using Chemical Film, yellow as per MIL-C-5541 followed by Black Anodized per MIL-A-8625 / MIL-PRF-8625
[⇦ this spec on DLA], TYPE II, CLASS 2 in USA so that we can work with them from Singapore,
Thank you.
- SINGAPORE