Good morning all,

I would like to know what kind of tests is recommended for vacuum vapor deposition of Cr (1st layer) and then Ni (2nd layer). The substrate is a lime glass. The metallization is at the edges of the glass. We are using a cellophane tape (L-T-90) for an adherence test. We look for no removal of the metallized coating from the glass edges. Is this test too agressive?. If so, how can we measure adhesion?

MIGUEL QUEVEDO
L-3 COMMUNICATIONS- EDI - ROLLING MEADOWS, IL, USA