Our metal levels in our Ni baths and Acid Cu baths rises and they need cut pretty regularly , on average about once every 4 months. I know that we should be able to reduce our anode area to lower the amount of metal build up but its just not a practical solution our problem.

I was wondering if its possible to use Titanium or Graphite anodes as auxialliries but hang them next to our normal anode baskets to help lower the metal content of the solution.

J. Ott
Plating Shop - Hbg, Pennsylvania


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search