Dear sir,
I am researcher and have hobby to electroplate aluminum (quite uncommon)with bright silver. I think aluminum will require copper plating then nickel plating and then bright silver route to be follow. am write?please guide me urgently.
bye.
have a nice day.
- India
++++++
Aluminum requires zincating. Then the copper - nickel - silver plating that you foresee.
The next person requesting "urgent!" help will get a bill for 50 cents. And we'll get back, in turn, a response: "I certainly didn't mean THAT urgent" :-)
|