Letter 42018 Pretreatment for powder coating on MS sheet [India]August 25, 2006 Sir, HRISHIKESH TA
August 25, 2006 Hi, Hrishikesh. You need to retain a consultant for this
pretreatment, or align yourself with a proprietary supplier who will
help you, or at least get hold of a book or two on pretreatment such
as Samuel Spring's
"Preparation of Metal for Painting
There are numerous approaches to pretreatment ranging from iron phosphate to zinc phosphate to proprietary modified phosphates to zinc plating to electropriming, and each of these has numerous variations. Unfortunately there is no way to say which is most appropriate for your situation without a detailed study. Good luck.
Dear Reader: please choose what you want to do--
![]() |
|
Save