-----Seeking finisher for MIL-P-53084 in Chicago area
2006
paint spec. reads "Cataphoretic Dip Paint (CDP), Black, thickness
20+5 microns. Coating material according MIL-P-53084, "Primer, cathodic electrodeposition Chemical agent resistant" Powercon 645 resin from PPG England.
We first need a five piece sample for qualification and then 10,000 pieces annually in 2500 piece lots.