Will anodizing (black) a welded miter in 6063-T52 result in uneven color?  

++++++

I have reviewed many "how to" postings and decided to hire the anodizing out at this time. The welding will also be hired out so wire selection is an open variable.

I want a perfect surface and am also concerned that even if the color is equally dark the light reflection off the extruded aluminum will be different then off of the welded surface. I could wet sand the entire surface before anodizing to get a uniform texture but am concerned that the extruded "texture" is what results in the satin quality that I want and sanding will negate that effect. Powder coating may be a better choice but I prefer the "satin" quality of anodized surfaces.

Thought I would see what others have to say before paying and being disappointed.

Nathanael Martin
Artist-hobbyist - Seattle,WA, USA


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com