Restoring a Copper Sink

++++++

I cleaned a copper sink but didn't realize it had a varnish. Unfortunately it sort of ruined it. I would like to get it back to the copper brown it was and then protect it again. Would you have a suggestion as to an inexpensive way to do this--ie. names of products or how to do a home remedy? I saw that I could buy a chemical called Tricolor Brown from a company for a mere $78 per gallon...not really worth it for me. I'm not sure if there is a good clear lacquer that would last. I'd appreciate any help.

Boosara Goldin
Consumer - San Diego, California, USA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search