Powdercoat peeling

   

++++++

I had an automatic pool cover installed last fall and the coating is peeling off the aluminum track and box cover as though it was painted....the finish looks different from the powdercoating finish on my patio furniture and I don't understand why.

Judith A. Jacoby
Homeowner - Middletown, New Jersey


++++++

Dear sir,
First thing powder coating peeloff has folowing main reason:-
1.Poor pretreatment(Chromatizing prefered for Aluminium object), it is not properly degreased.
2.Poor powder coating baking that means under baking.
3.Their may be powder problem.
Second thing when powder is peeling thats why it is finish not look like o.k.
Thanks
With regards,

Sanjay kumar Jain
- INDIA


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search