-----What is Electrostatic Spraying used for?
1999
My name is Chris
I am looking for information on electrostatic spraying. I want to know what it is mostly used for. I am looking for companies in my area that do this type of work. Or if you have a suggestion on what is good for wrought iron painting
thanks - Chris
Chris A. Maresjeweler - Tucson Arizona
Hi, Chris. Electrostatic spraying just means that paint or powder is sprayed onto a part that has been electrostatically charged to attract the paint or powder. The advantage is less waste to overspray.
You can look in our Shops Directory or your local yellow pages for painting or powder coating shops.
Regards,

Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
Need quick confidential answers? $25
Need project assistance? $100/hr.
March 6, 2009
Sorry! Finishing.com is temporarily Read-Only.
Ted Mooney is retiring but I have several offers to take it over.
We're working hard to make sure we find it the best new home.