Preparation of stainless steel prior to plastering 

-

I need to plaster over a stainless steel plate. Dimensions 50 mm x 1.3 m. I would be grateful for anybody's advice as to the correct preparation of the steel Thank you & Regards. Neil Franks

Mr Neil franks
- London, England


-

Hello Mr. Neil Franks,

The plaster will not stick directly to the steel (except by encapsulation). To deal with temp changes and high relative humidity, you will need to apply sheet rock (and maybe a moisture barrier) or metal lath to the steel for the plaster to mechanically adhere.

Regards,

Fred Mueller, CEF
- Royersford, PA


Dear reader

Post an answer
 
Post a question
 
Report broken links

 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com