Our customers require us to assemble Powder Coated parts.
Sometimes they are pitted or damaged. Is there a way to touch-up
Powder Coating or Handling defects?
A. Korselman
- San Francisco, California
-
Dear Mr A Korlselman,
This query has been answered by me on an earlier letter but at the
risk of repeating myself here goes:
Dissolve the same powder used in the coating in TC or any NC based
thinner in which the powder dissolves. Touch up the scratched area
with the resultant Paint /paste/ liquid powder whatever you call it
with a suitable paint brush.
Experience will give you an idea of how much your Solvent/ powder
mix should be.
All the best,
regards, K Vahanwala
|