Repolishing the black spot on titanium coated stainless steel sheets which is observed on time of welding [India] 

March 26, 2006

Interested to give us technical information for repolishing the black spot on Titanium coating on stainless steel which is observed on welding of sheets. And also information regarding the life of finishing of Titanium coating on sheets in exterior & interior.

Ramesh Shah
Patterned Stainless Steel Sheet & Tiles Specialist - Mumbai, Maharashtra, INDIA


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     