Salt spray resistance for E D

++++++

Hello every one,

what is the salt spray resistance for electro deposition coating?whether salt spray resistance is dependent on the dry film thickness?


thank you,

B SATHYA NARAYANAN
COLORSINDIA - CHENNAI, TAMILNADU, INDIA


++++++

The actual salt spray test results depend upon the substrate, the quality of phosphating and Electrocoating.

The salt spray specifications given by paint suppliers in India for Cathodic Epoxy Electrocoat on standard test panels when tested in compliance with the test standard ASTM B-117 [link is to spec at TechStreet] is 1000 hours.

Hope this answers you question.

Gurvin Singh
Coatec India -

Mohali, Punjab, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search