Recently purchase a nice antique dove tailed copper tea
kettle. However, it has a big ugly appearance problem.
Sometime long ago it appears someone did a very sloppy
retining of it's interior. Question: How do I get the messy
tin off exterior copper's surface? Thanks for any help!
Gloria Bowman
- Overland Park, Kansas
March 29, 2006
Try mixture of 1 part water/1 part
Muriatic Acid [link is to product info at Amazon]
(conc.), 65 C temp.
Good luck!