Letter 40043

Hot-corrosion related problem  

++++++

Why hot corrosion shows a linear axidation rate?

Dr. Syed Khalid Hasan
Faculty in an Engg. College - Gorakhpur, UP, India


I don't quite know what you mean. Are you saying that the hot corrosion rate is directly proportional to absolute temperature irrespective of the metal involved?


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey