During the purification of copper (through the process of electrolysis of copper sulfate) where dooes the sulfur and water (H20) go? Please help me! (year 11)

Lazar P.
- Perth, Western Australia, Australia


June 25, 2007

They just stay where they are, Lazar. The copper is electroplated out of solution and the sulfate and water remain in the solution.