Blue coloration on stainless steel when subjected to heat [India] 

March 24, 2006

I wish to know what temperatures stainless steel pipe of grade AISI 316L has reached if blue spots are observed on pipe when it is subjected to heat in limited air atmosphere for a duration of 75 minutes.

ABHIJEET NANDEDKAR
MANUFACTURING - BHILAI, CHATTISGARH, INDIA


March 24, 2006

This is one of the weirdest thermometers I've ever heard of, Abhijeet :-)

Please provide the background and why you want to know. Thanks and good luck!


Ted Mooney, P.E. 
finishing.com
Brick, NJ


April 2, 2006

Hi Abhijeet,

I am sure you will find the answer at the Nickel Institute. Check out their web page www.nickelinstitute.org.

Have fun,

Tony Johnston
- Doncaster East, Melbourne, Australia


Dear Reader: please choose what you want to do--

I want to answer or follow-up on this subject publicly (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
I want to post a new question or inquiry of my own on a different subject.
 





     

 Save This Page (why?)    -    Home    -    ©1995-2008 finishing.com