Hi
I have a problem with H202. I have dissolved copper and gold in H202 dropping the copper is easy enough but I was wondering if anyone had any ideas on on getting the gold out of it.

I have several gallons of this stuff and hate to see it go to waste, any suggestions?

Brian Powell
Hobbyist - Virginia, USA


++++++

How do you disolve gold in peroxide?? Some will drop out if you kill the peroxide. Sugar will do that. Boil it down is another way. Be careful of this as peroxide reaches a temperature where it generates so much heat that the reaction becomes faster and faster yielding bubbles all over the place. vacuum evaporation will work if you have a vacuum source. Slow but safe. There are a couple of organic compounds that will drop out gold as a sponge. Have not seen it in print in a couple of years tho.

James Watts
- FL


Dear reader

Post an answer
 
Post a question
 
Report broken links


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com