Letter 39477

Tin plating copper parts with stainless (sus 302/303) hardwares, any problem?  

February 15, 2006

We are in sheet metal fabrication. We have copper parts with stainless PEM parts(self-clinching nuts) attached on it. Is it ok to tin plate the parts after the nuts are inserted? What problem may arise with this process.

Thanks for any clarification.

Don Mar
Sheet Metal Fabrication - Bangkok, Thailand


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button


List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com