Home of the finishing HOTLINE since 1989

-----

Need powder to meet Ford WSS-M2P180-A / WSS-M2P90 powder coating spec




2005

Hello, all:
Right now I'm looking for a powder coating to meet Ford WSS-M2P180-A spec. The color should be YGYAXXG or M6388G. The gloss after coating should be 20 ±3. I contacted Rohm & Haas and Dupont; neither has a product to meet that spec.
If you have some information about that, please advise.

Thanks a lot.

Woodear S [last name deleted for privacy by Editor]
auto parts manufacturing - Windsor, ON, Canada

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).



Q. Has anyone answered this question? Am I correct that the spec was updated in 2011 to WSS-M2P90? Any suggestions on which powder coat material will meet the 480-hour salt spray spec?

Jeff Peck
- Bloomfield Hills, Michigan USA
November 3, 2016


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"