finishing.com -- The Home Page of the Finishing Industry Search our quarter-million Q&As

Home of the finishing HOTLINE since 1989

-----

Electropolishing



Q. I am trying to electropolish Stainless Steel (Inox). I have added all the different acids but not sure on the Qty per acid. I am getting a matte like shine not a bright finish.

Brett Authers
Bull bars - South Africa
2005


A. That sounds like "etching", which is very common in electropolishing if anything is out of the suggested range. Especially, it is universal if the current density is too low. What is your current density, and what acid concentration are you actually running?

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2005


A. The matte finish sounds like 'frosting' to me. This sometimes happens with a lack of current or poor pre-treatment. Make sure the surface is very clean and free from oxides. I can't remember off the top of my head but I think a solution of about 60% Phosphoric acid, 30% Lactic acid and 10% sulfuric acid is about right. Give the parts about 10V for 2-3 minutes.

Chris Matthews
- East Sussex, England
2005



Q. Dear friends, I want to know the material of the pads used in the Electropolisher's Anode?

Ranjit V Srivatsaa
- Chennai, India
2005




Q. Is there a standard or a specification for electropolishing?

Bill Rooney
- Milford, Massachusetts
2005


A. Hi Bill. ASTM B912 is a general one, Bill. But there are others for some particular industries, and there may even be one covering the particular industry or type of parts in question. Please expound on your situation. Thanks.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.
2005


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"