| Search our quarter-million Q&As |
Home of the finishing HOTLINE since 1989
-----What is a Chrome 40 finish?
Can you tell me what is a "chrome 40 finish" ?
Joe Schmitt- Croydon, Pennsylvania
1999
The only thing that come to my mind is process named Econochrome 40 for hard chrome plating based on fluorides.

Sara Michaeli
Tel-Aviv-Yafo, Israel
1999