Need Nickel and Hard Chrome Plating on Long cylindrical Parts
+++++I am searching for a vendor who has the capacity to plate both nickel and hard chrome on a fairly long component. Specifically we have a part that is approximately 26 feet in length with an OD of 19" in diameter. The part is approximately 5500 lbs.
Fife EllisOil Field Manufacturer - Houston, Texas
----