Letter 37041
Which test for low performance plating on
Steel parts? [Singapore]
+++++
Hello,
I need to specify a test, that if passed would garantee that the
parts will be able to remain White rust free after 2 years in an
indoor environement (up to 95% humididty)
I tried some salt mist but 72 hours seems too severe.
Any recommendations ?