Letter 36029

Gun bluing trouble  

+++++

What is the correct formula of hot caustic bluing for making up a bluing bath for refinishing guns, and can we regenerate the bath again and again , and how can we extend the life of the bath, as I am making the bath in the following manner:
caustic soda 10 kg
sodium nitrate 10kg
water 10 liters.
The bath forms red cast on the parts which is easily rubbed off but the bath lasts only an hour or so,please advise.

Inderjit Sidhu
firearms - Patiala, Punjab, India


+++++

Hi Inderjeet,

Forget about your formula search and buy the correct readymade product from any reputed company in your country.

Khozema Vahanwala
Saify Ind
 
Bangalore, Karnataka, India


++++++

Wath is de formula for gun blue hot cauistic blueing for home make, I want bluing my gun is old and has rust
thanks,,

Santi Salinas
- Quito, Ecuador


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com