Brightener for alkaline zinc-iron plating




2005

I am Mona Moayeri, Student(m.s), from Univ of Tehran.
My question is about brightening of zinc-iron plating in alkaline bath.
tnx a lot
have a great day

Mona Moayeri
univ of tehran - Iran



Sorry, Mona, I am not aware of any zinc-iron plating processes that are not proprietary.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha
finishing.com - Pine Beach, New Jersey
2005



Hello Miss Moayeri!
I am a metallurgy engineer from amirkabir uv. I research phosphating bath-zinc electroplating bath(cyanide)and it's brightener-alloy electroplating- chromating bath (yellow- blue-green-black). The brightener of alkaline zinc bath consist of very compound like alcohols, carboxylic acids, glucose, vanillin, and other materials.the canning company is the best in brightener.

Amir Khakzad
zinc electroplating - Tehran
2005




(No "dead threads" here! If this page isn't currently on the Hotline your Q, A, or Comment will restore it)

Q, A, or Comment on THIS thread -or- Start a NEW Thread

Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2024 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"