I want to procure two anodizing rectifers -- one for hard anodizing and one for simple anodizing. The spec of rectifiers are as follows.
hard anodizer, input 480 volts out put 20 -100 volts 1000 amp
simple anodizing input 480 volts out put 10-25 volts and 1000 amp\
both may be oil cooled.
further equipment I want to procure are anodizing chiller and anodizing process tanks qty 02 one for hard anodizing and one for simple anodizing. I could not get such info from any where so there fore I request you to send me valuable information regarding this issue.
regards

Mahboob Alam
A.E.R.O - WAH CANTT,PAKISTAN



----
Readers: This site is made available for camaraderie & technical info exchange by our supporting advertisers, and they will contact the inquirer privately regarding their commercial needs. Please offer comments on any technical issues, but not sourcing suggestions or testimonials. Thanks!


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search