Electropolishing of copper in orthophosphoric acid solution

+++++

Hi, I need your help to find a theoretical data about electropolishing of copper, I need it to finish my graduation project, I've done my experimental part of the project, the main aim of my project is to find the effect of concentration, anode diameter & temperature on the limiting current so the rate of electropolishing.
Electropolishing of horizontal copper cylinder in orthophosphoric acid.

Joe Elshamy
Alex. university, Faculty of engineering - Alexandria, Cairo


+++++

With the experimental work done, what results did you get, Joe?

You probably now need to do a computerized search of the published literature. But I see on the net a reference to an article "Electrolytic polishing of copper in orthophosphoric acid", (Australia. Council for Scientific and Industrial Research. Division of Tribophysics. Physical metallurgy report) by R. W. K Honeycombe, and maybe you can track down a copy of that. There is a lot about electropolishing, but only a little about electropolishing of copper, in ASM Metals Handbook Vol. 5 "Surface Engineering" and the Electroplating Engineering Handbook. Good luck!


Ted Mooney, P.E. 
finishing.com
Brick, New Jersey

 

 


Dear reader

Post an answer
 
Post a question
 
Report broken links

 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com