Need heat resistant powder for coating silencers of tractors


RFQ: We need heat resistant black powder for coating on silencers to be used on tractors. Should be able to withstand temperature up to 500+ °C. Bulk quantities may be required for use on regular basis.

Please intimate addresses of suppliers in the business of powder paints.

Subhash Sikka
automotive silencer manufacturing - Chandigarh, India
2004

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).



RFQ: We need heat resistance black powder for coating on silencers to be used on tractors. Should be able to withstand temperature up to 500 plus °C. the bulk quantities may be required for use on regular basis.

Please intimate addresses of suppliers in business of powder paints.

Peter Pereira
- Ghatkopar, Maharashtra, India
2005

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).



RFQ: We are in the line of powder coating process. We need powder paint for coating of silencers of vehicles like tractors, motorbikes, etc. Also complete information on this process.

Sunil R PETHE
- Pune, India
2005

Ed. note: This RFQ is outdated, but technical replies are welcome, and readers are encouraged to post their own RFQs. But no public commercial suggestions please ( huh? why?).


Ed. note: Current RFQs can be found on our "Looking for a Product or Service for Our Finishing Shop" page.


A. I doubt that you will be doing this with powder, do these silencers fit on the end of the tail pipe? If they do, you'll probably end up switching to a high temperature header paint.

Sheldon Taylor
Sheldon Taylor
supply chain electronics
Wake Forest, North Carolina

2005


A. There are heat resistant powders available in India too sufficient to meet stringent requirements like heat quenching cycles. However, the usage is less due to higher price. Look at the best paint companies to recommend to you.

Amit Amembal
- Mumbai, India
2006


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"