Need help on thick high purity Rhodium film  

+++++

I need to know if pure rhodium up to .001" thick can be deposited onto small molybdenum disks ( 2" by .250" thick, edge only. I know that it will be pricey. Would electroplating eventually work without becoming too nodular? How about vacuum arc or other methods?

Jim Burke
baggage bomb detection - Salt Lake City, UT, U.S.A.


Dear Reader, please --

Answer or follow-up on this subject (in non-commercial fashion).
 
My company is a supporting advertiser at finishing.com and we want the contact information to reach the inquirer privately.
 
Post a new question or inquiry on a different subject.
 


Legal disclaimer boilerplate button

List of Directories
Jobshops Directory button Environmental Directory button Equipment Directory button Consultants Directory button Chemicals Directory button Test Directory button Help-Wanted Directory button About Advertising button Classifieds Directory button Booklist button

 

Link to Del.icio.us button Save This Page (why?)    -    Home    -    ©1995-2009 finishing.com