Roughness as per Sa 2 1/2
++++
For the preparation of CS surface I need to know the grit profile from blasting as per Sa 2-1/2 (roughness). Thank you in advance for your prompt answer.
Omar KhericiOil and gas project - Almaty, Kazakhstan
September 3, 2009
what is Sa 2 1/2 regarding surface preparation. and Sa stand for what?
dushyant upadhyay- varansi, u.p., India
September 3, 2009
Hi, Dushyant. This is a Swedish Institute for Standards designation for "near white" blasted finish -- approximately equivalent to NACE No. 2/SSPC-SP10 [link is to spec at TechStreet] 2, and ISO 8501-1 [link is to spec at TechStreet] WA.2.5
I believe it's actually "Sa.2.5", but I don't know is "Sa" is an abbreviation or acronym in Swedish.
Please see letter 12526 for a more complete explanation.
Regards,
|
Ted Mooney, P.E. RET finishing.com Brick, New Jersey |