Brazing zinc plated parts


(2004)

I have a zinc plated part that I that will be brazed onto a mating part that is not zinc plated. Will the brazing process cause the zinc plating to break down or come off the part?

Vito De Monte
E-Z-EM, Inc. - Westbury, New York, USA


(2004)

Both.

khozema
Khozem Vahaanwala
Saify Ind supporting advertiser
Bangalore, Karnataka, India

saify logo

ADD a Q or A to THIS thread START a NEW THREADView This Week's HOT TOPICS

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

  If you need a product/service, please check these Directories:

JobshopsCapital Equip. & Install'nChemicals & Consumables Consult'g, Train'g, SoftwareEnvironmental ComplianceTesting Svcs. & DevicesUsed & Surplus


©1995-2017 finishing.com     -    Privacy Policy
How Google uses data when you visit this site.