Metal finishing Q&As since 1989
-----
Which media for stripping paint off car
What kind of plastic can I use to sandblast a car I'm restoring?
Thanks,
Jerry Barrow
metal stripping - Lebanon, Tennessee, USA
2004
The glass small spheres, 0,2-0,5mm dia will be the best for you.
Damian Dinu
Constanta, ROMANIA
2005
Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.