General description of Tin Plating process


1999

Dear Sir;

Can you direct me to a web page that gives a general description of the tin plating process? I am especially interested in immersion plating for parts and reel-to-reel plating of coils of copper tubing. Can you help?

Thanks,

David Hicks



I don't think the web is the place to start, Mr. Hicks. You'll learn a lot more, and much faster, from books. The way things are organized in most writers' minds, you are asking for info on three different subjects actually: tin chemistry, immersion plating, and reel-to-reel systems. I would suggest you get hold of the Metal Finishing Guidebook and the Electroplating Engineering Handbook this on eBay, AbeBooks, or Amazon [affil link] , described in more detail on our "must-haves" booklist.

Ted Mooney, finishing.com
Ted Mooney, P.E.
Striving to live Aloha

finishing.com - Pine Beach, New Jersey

Need quick confidential answers? $25
Need project assistance? $100/hr.


Sorry! Finishing.com is temporarily Read-Only.
Please maintain your bookmarks! Although Ted Mooney is retiring, finishing.com is not!
It will have a new owner/curator very shortly!



Disclaimer: It's not possible to fully diagnose a finishing problem or the hazards of an operation via these pages. All information presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The internet is largely anonymous & unvetted; some names may be fictitious and some recommendations might be harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Finishing
Jobshops
Capital
Equipment
Chemicals &
Consumables
Consult'g,
& Software


About/Contact  -  Privacy Policy  -  ©1995-2026 finishing.com, Pine Beach, New Jersey, USA  -  about "affil links"