We passivated at high temp, will it be a problem?

++++

Hi everyone,

I have a batch of SUS302 metal split pins that were passivated at 72 degree celsius. The recommended temperature is 49-54 degree celsius. Is there any effect on the pins due to the increase in temperature?

SN Seah
Contract Manufacturer - Singapore


++++

I am not a metallurgist but I assume "not really".

khozema Khozema Vahanwala
Saify Ind
 
Bangalore, Karnataka, India


ANSWER or FOLLOW UP POST an unrelated QUESTION HOT Topics

Disclaimer: It is not possible to diagnose a finishing problem or the hazards of an operation via these pages. All information
presented is for general reference and does not represent a professional opinion nor the policy of an author's employer. The
internet is largely anonymous; some names may be fictitious and some recommendations may be deliberately harmful.

If you are seeking a product or service related to metal finishing, please check these Directories:

Jobshops Capital Equip. & Install'n Chemicals & Consumables Consult'g, Train'g, Software Environmental Compliance Testing Svcs. & Devices Used & Surplus


Home    -    Contact    -    ©1995-2012 finishing.com     -    Privacy    -    Search